[1]邱俊明,蒋柏泉*.CuO-CeO2/CSAC催化剂制备及其处理染料废水[J].江西师范大学学报(自然科学版),2020,(06):584-589.[doi:10.16357/j.cnki.issn1000-5862.2020.06.06]
 QIU Junming,JIANG Boquan*.The Preparation of CuO-CeO2/CSAC Catalyst and Its Treatment of Dyeing Wastewater[J].Journal of Jiangxi Normal University:Natural Science Edition,2020,(06):584-589.[doi:10.16357/j.cnki.issn1000-5862.2020.06.06]
点击复制

CuO-CeO2/CSAC催化剂制备及其处理染料废水()
分享到:

《江西师范大学学报》(自然科学版)[ISSN:1006-6977/CN:61-1281/TN]

卷:
期数:
2020年06期
页码:
584-589
栏目:
化学与环境科学
出版日期:
2020-12-20

文章信息/Info

Title:
The Preparation of CuO-CeO2/CSAC Catalyst and Its Treatment of Dyeing Wastewater
文章编号:
1000-5862(2020)06-0584-06
作者:
邱俊明12蒋柏泉2*
1.南昌大学期刊社,江西 南昌 330031; 2.南昌大学资源环境与化工学院,江西 南昌 330031
Author(s):
QIU Junming12JIANG Boquan2*
1.Periodical Press,Nanchang University,Nanchang Jiangxi 330031,China; 2.School of Resources, Environmental and Chemical Engineering,Nanchang University,Nanchang Jiangxi 330031,China
关键词:
氧化铜 活性炭 二氧化铈 湿式催化氧化 染料废水 金属催化剂
Keywords:
copper oxide activated carbon cerium dioxide wet catalytic oxidation dyeing wastewater metal catalyst
分类号:
X 703
DOI:
10.16357/j.cnki.issn1000-5862.2020.06.06
文献标志码:
A
摘要:
用自制的椰壳活性炭作为载体制备CuO-CeO2/CSAC催化剂处理酸性大红GR染料废水.正交实验优化了CuO-CeO2/CSAC制备的工艺参数,单因素和响应面联合实验优化了CuO-CeO2/CSAC处理酸性大红GR废水的工艺条件.实验结果表明:CuO-CeO2/CSAC的最佳制备工艺参数为τ=2.50 h,T=300.0 ℃,V1=15.0 mL,V2=5.0 mL,其对CODCr和色度的降解率比单组分CuO/CSAC催化剂分别提高了62.4%和69.7%.CuO-CeO2/CSAC在室温下处理模拟废水的最佳条件为τ=4.12 h,m=0.57 g,pH值为5.0,可将CODCr和色度分别从 962.0 mg·L-1和32 720.0倍降解至35.2 mg·L-1和12.7倍,相应的降解率为96.30%和99.96%.建立的分别以CODCr和色度残余质量浓度为响应值的工艺模型与实验结果吻合较好,可预测不同工艺条件下降解CODCr和色度的效果.
Abstract:
CuO-CeO2/CSAC catalyst is prepared by using self-made coconut shell activated carbon as carrier to treat acid bright red GR dye wastewater.The preparation parameters of CuO-CeO2/CSAC are optimized by orthogonal experiment.Single factor combined with response surface experiment are used to optimize the processing conditions of the treatment of acid scarlet GR wastewater by the prepared CuO-CeO2/CSAC catalyst.The results show that the optimum process parameters of the CuO-CeO2/CSAC preparation are τ= 2.50 h,T= 300.0 ℃,V1=15.0 mL,V2=5.0 mL,and its degradation rates of CODCr and chromaticity are 62.4% and 69.7% higher than those of single component CuO/CSAC catalyst.The optimal condition for treatment of simulated wastewater by CuO-CeO2/CSAC at room temperature are τ=4.12 h,m=0.57 g,pH=5.0,and the CODCr and chroma are degraded from 962.0 mg·L-1 and 32 720.0 times to 35.2 mg·L-1 and 12.7 times,respectively.The established process models with CODCr and chromaticity residual concentration as the response values are in good agreement with the experimental results,which can predict the effects of CODCr and chroma degaradation under different process conditions.

参考文献/References:

[1] 王栗,岳琳,郭建博,等.FePMo12催化电化学反应降解染料废水的研究[J].环境科学,2018,35(5):1843-1849.
[2] 周自成.过渡性金属氧化物的制备及其对亚甲基蓝的吸附和催化性能研究[J].沧州师范学院学报,2017,33(2):43-48.
[3] Ji Xiaoxu,Bai Chongchong,Zhao Qinghuai,et al.Facile synthesis of porous SnO2 quasi-nanospheres for photocatalytic degradation of Rhodamine B[J].Materials Letters,2017,189:58-61.
[4] Navarro P,Gabaldón J A,Gómez-López V M.Degradation of an azodye by a fast and innovative pulsed light/H2O2 advanced oxidation process[J].Dyes and Pigments,2017,136:887-892.
[5] Wang Xurong,Yang Wenzhong,Ji Yan,et al.Heterogeneous Fenton-like degradation of methyl blue using MCM-41-Fe/Al supported Mn oxides[J].RSC Advances,2016,6:26155-26162.
[6] Wang Yan,Gao Yaowen,Chen Lu,et al.Goethite as an efficient heterogeneous Fenton catalyst for the degradation of methyl orange[J].Catalysis Today,2015,252:107-112.
[7] Rusevova K,Köferstein R,Rosell M,et al.LaFeO3 and BiFeO3 perovskites as nanocatalysts for contaminant degradation in heterogeneous Fenton-like reactions[J].Chemical Engineering Journal,2014,239:322-331.
[8] Mu Guangyu,Wei Qinglian,Huang Yongmin.Facile fabrication of CeO2 hollow microspheres with yeast as bio-templates[J].Journal of Rare Eearths,2015,33(12):1329-1334.
[9] Gu Yu,Liu Chuntao,Li Yabei,et al.Ce0.8Sn0.2O2-δ-C composite as a co-catalytic support for Pt catalysts toward methanol electroxidation[J].Journal of Power Sources,2014,265:335-344.
[10] 李红梅,张云峰,梅英,等.介孔二氧化铈纳米材料的制备与性能[J].稀有金属材料与工程,2015,44(5):1269-1272.
[11] Wang Li,Ding Jing,Chai Yuanyuan,et al.CeO2 nanorod/g-C3N6/N-rGo composite:ethanced visible-light-driven photocatalytic performance and the role of -N-rGo as electronic transfer media[J].Dalton Transactions,2015,44(24):11223-11234.
[12] Lin K S,Chowdhury S.Synthesis,characterization,and application of 1-D cerium oxide nanomaterials:a review[J].International of Journal Molecular Sciences,2010,11(9):3226-3251.
[13] 靳广洲,殷慧玲.氧化铈对负载型氧化铜催化剂的助催化作用[J].石油大学学报:自然科学版,1997,21(2):76-78.
[14] 柯鹏,袁丁,刘义清.CeO2改性微波诱导催化剂CuO/γ-Al2O3催化氧化处理偶氮染料废水[J].化学工程师,2008,22(6):24-26.
[15] 蒋柏泉,曾芳,曾庆芳,等.废椰壳制备活性炭负载CuO处理活性艳红X-3B废水的工艺优化[J].环境工程学报,2013,7(9):3284-3288.
[16]刘玉德,蒋柏泉,陈建新.椰壳制备活性炭负载氧化铜处理酸性大红GR染料废水[J].南昌大学学报:工科版,2011,33(3):222-226.

备注/Memo

备注/Memo:
收稿日期:2019-05-01
基金项目:国家自然科学基金(20807020)资助项目.
作者简介:邱俊明(1976-),男,江西南康人,副编审,主要从事环境化工研究.E-mail:qiujunming@ncu.edu.cn
通信作者:蒋柏泉(1949-),男,江苏无锡人,教授,主要从事环境化工研究.E-mail:jbq_win@163.com
更新日期/Last Update: 2020-12-20